双组分聚氨酯防水涂料.jpg

product overview

one-component polyurethane waterproof coating is a kind of wet curing waterproof coating, which can be directly applied on wet base surface, and can be coated once to form a high elastic waterproof layer. the film has strong adaptability to cracking and expansion of base.

scope of application of products

the product can be used for waterproofing construction of roof, basement, toilet and bathroom, swimming pool and other civil and industrial construction projects. it is suitable for waterproofing construction of various complex shapes and vertical and horizontal pipelines.


product construction

step one:

in the treatment of grass-roots, the grass-roots should be firm, flat, free of impurities, fully dry, and the yin-yang angle should be circular arc, with the diameter of yin-yang angle greater than 50 mm and the diameter of yang-angle greater than 10 mm.

step two:

ingredients and dosage: according to construction dosage, single component open cover mixing can be used evenly. reference dosage: 1 mm thick film dosage is about 1.3-1.5 kg/m2.

step three:

large-area waterproof construction: uniform coating with rubber or plastic scrapers, requiring uniform thickness, generally 1.5mm-2mm, should be divided into 3-4 times of painting, the next painting should be solidified after the previous painting, and be painted in a vertical direction, generally as a separate film, the floor of underground engineering should be coated with a layer of matrix reinforcement material.

step four:

coating film thickness: underground engineering is 1.2mm-2.0mm, generally 1.5mm, toilet bathroom is not less than 1.5mm. when exposed roof engineering adopts multi-channel waterproofing, the thickness of each channel is not less than 1.2mm. when waterproofing grade is iii roof, waterproofing thickness is not less than 2mm. when adding matrix reinforcement material between layers, the thickness of the layer below the matrix. no less than 1.0mm and the top layer is no less than 0.5mm.

step five:

finishing layer construction: scatter clean sand on the surface before brushing the last time the paint has not solidified.

step six:

protective layer: the surface of the waterproof coating should be insulated according to the design requirements.


one-component oily polyurethane waterproof coating 2019-8-16 this article is read 604 second
prev:delivery sitenext:delivery site








logo1.png

凯发ag旗舰厅 copyright©:weifang tianyuan waterproof material co., ltd.  
网站地图